Boley #1 non-magnetic superalloy watchmaker tweezers 120mm
Boley #1 non-magnetic superalloy watchmaker tweezers 120mm
Boley #1 non-magnetic superalloy watchmaker tweezers 120mm
  • Load image into Gallery viewer, Boley #1 non-magnetic superalloy watchmaker tweezers 120mm
  • Load image into Gallery viewer, Boley #1 non-magnetic superalloy watchmaker tweezers 120mm
  • Load image into Gallery viewer, Boley #1 non-magnetic superalloy watchmaker tweezers 120mm

Boley #1 non-magnetic superalloy watchmaker tweezers 120mm

Regular price
£30.13
Sale price
£30.13
Regular price
Sold out
Unit price
per 

Boley non-magnetic tweezers in Ni-Cr-Mo superalloy, comparable to Taxal quality. The Boley Superalloy Tweezers are six times harder and more resistant than conventional non-magnetic stainless steel tweezers.

Features:
- Nickel-Chromium-Molybdenum (Ni-Cr-Mo) superalloy
- excellent/resistance to room temperature up to 800°C
- 100% non-magnetic and even six times harder than antimagnetic stainless steel tweezers
- resistant to fatigue, very high shape retention
- excellent corrosion resistance to most chemicals, salts and acids
- comparable to Taxal quality

Type: No. 1
Execution: Strong points
Length: 120mm
Material: superalloy